Q:- For procedure qualification, the exposed surfaces of each nick-break specimen shall show:

1. No slag inclusions over 1/4 inch 
2. At least 3/4 inches of sound weld metal between inclusions 
3. Complete penetration and fusion 
4. The tensile strength of the sample 

Sunday, 2 April 2017

Q:- For welder qualification, the specimens shall be prepared for tensile-strength, nick-break, and bend tests. When tensile-strength tests are omitted:

1. The welder is not qualified 
2. The weld must be redone 
3. The is not covered in API 1104 
4. Tensile-Strength specimens shall be subject to the nick-break test 
5. Extra face bends must be tested

Thursday, 7 July 2016

Q:- Atmospheres for shielding an arc may consist of:


1. Inert gases, active gases, or mixtures of inert and active gases 
2. Only inert gases are permitted 
3. Only active gases are permitted 
4. No gases are permitted for welding