- Flushed caps will always break in the weld metal area
- This is to remove any porosity in the excess weld metal (weld cap)
- It is easier to calculate the cross section areas of the joint when fused
- Flushed caps have fuser stress raisers and therefore give a more aqua rate result
Eurotech an authorized Agent of American Welding Society(AWS). We conduct AWS CWI Examination with documented training in INDIA and MIDDLE EAST. For More Information contact to Mr.Puneet Sharma E-mail: (aws.cwi.training@gmail.com)
Friday, 1 May 2015
Q:- Some codes require the excess weld metal (weld cap) on cross weld joint tensile specimens to be flush ground, this is because: