- A hydrogen level increase lamellar tearing which more likely
- As material thickness increase ductility decease making lamellar tearing more likely
- Lamellar tearing occur in a HAZ
- Lamellar tearing effect all type of joints
Eurotech an authorized Agent of American Welding Society(AWS). We conduct AWS CWI Examination with documented training in INDIA and MIDDLE EAST. For More Information contact to Mr.Puneet Sharma E-mail: (aws.cwi.training@gmail.com)